04/06 oxidation
Contributed by: Robert Saxby
Should be soaked for 30 minutes at temp to avoid pinholes. Commercial underglazes can be painted over. To make sure they flux add 25% 3124 to these.
![]() | 3124 Frit | ![]() | 100 |
![]() | Zircopax | ![]() | 25 |
![]() | China Clay | ![]() | 15 |
![]() | Barium | ![]() | 4 |