Cone 6 oxidation
Contributed by: Robert Saxby
Can be runny. This is a well known glaze.
![]() | Nepheline Syenite | ![]() | 48 |
![]() | Gerstley Borate | ![]() | 27 |
![]() | Flint | ![]() | 21 |
![]() | Edgar Plastic Kaolin | ![]() | 5.5 |
![]() | Rutile | ![]() | 3.5 |
![]() | Red Iron Oxide (FeO2) | ![]() | 2 |
![]() | Cobalt Oxide | ![]() | 1 |